MIXING AND
APPLICATION INSTRUCTIONS
WATER BASE EPOXY PRIMER
PRODUCT MIXING: This product comes prepackaged
by weight. Kits should be mixed in their entirety. After the two parts are combined,
mix well with slow speed mixing equipment such as a jiffy mixer until the material
is thoroughly mixed and streak free. This product is an emulsion product and
should be mixed well before using.
PRODUCT APPLICATION: The mixed
material can be applied by brush, roller or spray. Maintain
temperatures within recommended ranges.
DRY TIME: Light foot traffic, 16-24
hours at 70 degrees F.
CONCRETE PREPARATION FOR FLOOR COATING:
Acid etching solution will not work properly on greasy, oily, or
painted surfaces. This concrete must first be cleaned with
either, Northern Aqua-Blue or Northern Scrub-Free, for heavy film
buildup removal.
Acid solution should always start at lowest level of a floor,
usually the drains. Apply in a circular fashion out away from
drains. Remember acid solution will not work properly when poured
on "spent" or "used" acid solution. Acid
solution should "foam" or "froth" instantly
when poured on the concrete. Slow or no reaction is a sign the
concrete was not ready to be etched. Clean and repeat above
procedure.
Muratic and hydrochloric acids are available commercially at most
hardware or pool supply stores. Mix 2 parts water with 1 part
acid for good etching. Using a plastic watering sprinkler, apply
the mixed acid solution (always add water to the can first) at a
spread rate of 50 sq. ft. per gallon. Acid solution must be
"worked" into the substrate with a stiff bristle broom
to completely agitate the floor. Once acid solution stops
frothing (approximately 10-15 minutes) flush the remaining
solution to drain and rinse floor thoroughly. "Do not let
solution dry". Rinse floor a second time with some household
ammonia to neutralize any acid residue that might remain.
MIXING AND APPLICATION INSTRUCTIONS
MEGA-BUILD EPOXY
PRODUCT MIXING: This product has a
mix ratio of two parts A to one part B by volume. Standard
packaging is 3 gallon and 15 gallon units. After the two parts
are combined, mix well with slow speed mixing equipment such as
jiffy mixer until material is thoroughly mixed and streak free.
PRIMER: A suitable primer should be
used before applying this product. Northern waterbase epoxy is
recommended.
PRODUCT APPLICATION: The mixed
material can be applied by brush, roller, or spray. A serrated
squeegee may also be used, then backrolled with a roller to
smooth out the floor.
DRY TIME: Light foot traffic in
12-14 hours at 70 degrees F.
CONCRETE PREPARATION FOR FLOOR COATING:
Acid etching solution will not work properly on greasy, oily, or
painted surfaces. This concrete must first be cleaned with
either, Northern Aqua-Blue or Northern Scrub-Free, for heavy film
buildup removal.
Acid solution should always start at the lowest level of a floor,
usually the drains. Apply in a circular fashion out away from
drains. Remember acid solution will not work properly when poured
on "spent" or "used" acid solution. Acid
solution should "foam" or "froth" instantly
when poured on the concrete. Slow or no reaction is a sign the
concrete was not ready to be etched. Clean and repeat above
procedure.
Muratic or Hydrochloric acids are available commercially at most
hardware or pool supply stores. Mix 2 parts water to 1 part acid
for good etching. Using a plastic watering sprinkler, apply the
mixed acid solution (always add water to the can first) at a
spread rate of 50 sq. ft. per gallon. Acid solution must be
"worked" into the substrate with a stiff bristle broom
to completely agitate the floor. Once acid solution stops
frothing (approximately 10-15 minutes) flush remaining solution
to drain and rinse floor thoroughly. "Do not let solution
dry". Rinse floor a second time with some household ammonia
to neutralize any acid residue that might remain.